Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.390 - 0.600 GPa | 56.6 - 87.0 ksi | ASTM D638 |
Zeus PTFE Tubing Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,.. |