Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 270 °C | 518 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Middle Barrel Temperature | 270 - 320 °C | 518 - 608 °F | |
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Middle Barrel Temperature | 270 - 310 °C | 518 - 590 °F | Injection Molding |
LG Chemical LUCON CP6052 PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 275 °C | 518 - 527 °F | |
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
Middle Barrel Temperature | 270 - 275 °C | 518 - 527 °F | |
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester Vypet VNT 245 is a 45% fiberglass reinforced modified PBT / PET polyester injection molding compound designed for electrical and automotive applications requiring low warp and improved surface finis.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Middle Barrel Temperature | 270 - 290 °C | 518 - 554 °F | |
Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced Notes: ALF20 is a self-lubricating grade of nylon 66 containing PTFE and Silicone. It offers outstanding surface wear characteristics of molded parts. It is suitable for applications such as beari.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Middle Barrel Temperature | 270 - 310 °C | 518 - 590 °F | |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Middle Barrel Temperature | 270 - 320 °C | 518 - 608 °F | |
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |