Processing Properties Metric English Comments
Dry Time 3 - 5 hour
3 - 5 hour
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Dry Time 4 - 5 hour
4 - 5 hour
RTP Company RTP 285 K TFE 15 Polyarylamide (PAA), Carbon Fiber - PTFE Lubricated  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Dry Time 3 - 5 hour
3 - 5 hour
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Dry Time 3 - 5 hour
3 - 5 hour
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Dry Time 3 - 5 hour
3 - 5 hour
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Dry Time 3 - 5 hour
3 - 5 hour
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Dry Time 3 - 5 hour
3 - 5 hour
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Dry Time 3 - 5 hour
3 - 5 hour
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Dry Time 3 - 5 hour
3 - 5 hour
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3030I Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3030U Polycarbonate, UV Stabilized
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3025A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dry Time 3 - 5 hour
3 - 5 hour
Predrying Time
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Dry Time 3 - 5 hour
3 - 5 hour
Predrying Time
Tisan TISARBON® UNR Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Dry Time 3 - 5 hour
3 - 5 hour
Predrying Time
Tisan TISBLEND® PC/ABS
TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High..
Dry Time 4 - 5 hour
4 - 5 hour
Predrying Time
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Dry Time 4 - 5 hour
4 - 5 hour
Predrying Time
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Dry Time 3 - 5 hour
3 - 5 hour
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Dry Time 3 - 5 hour
3 - 5 hour
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Dry Time 3 - 5 hour
3 - 5 hour
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Dry Time 3 - 5 hour
3 - 5 hour
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Dry Time 3 - 5 hour
3 - 5 hour
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Dry Time 3 - 5 hour
3 - 5 hour
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr..
Dry Time 4 - 5 hour
4 - 5 hour
RTP Company RTP 203 K TFE 15 Polyarylamide (PAA), Glass Fiber - PTFE Lubricated  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Dry Time 4 - 5 hour
4 - 5 hour
RTP Company RTP 209 K Polyarylamide (PAA), Glass Fiber  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Dry Time 3 - 5 hour
3 - 5 hour
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant