Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory nature of silicone lubricants.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.80 %
0.80 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Flexural Yield Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 9.31 GPa
1350 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.15
0.15
Coefficient of Friction, Static 0.14
0.14
K (wear) Factor 604 x 10-8 mm³/N-M
300 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Limiting Pressure Velocity 0.420 MPa-m/sec
12000 psi-ft/min
at 100 FPM, ambient temperature, thrust washer.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
485 °F
ASTM D648