Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ PC GR30 Glass Reinforced Polycarbonate OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 22.8 °C |
2.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 6/6, 35% Fiberglass (DAM)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF33 L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackTPCI# 8221102Information provid.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature -30.0 °C |
2.19 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 LNP THERMOCOMP* PF006U is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of thie grade are: UV Stabilized. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN130GMD2 (DAM) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PC310GR Polycarbonate (Utility Grade), 10% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Diamond Polymers ABS TR-7 Description: High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S519 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436G15M15CL Glass/Mineral Reinforced Coupled |
|||
Izod Impact, Notched | 1.17 J/cm | 2.19 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 63M Nylon 66, Mineral Filled A mineral filled Nylon 66 providing superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-40FG-1804 40% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame RetardantFeatures: Flame Retardant UL File Number: E157318Processing Met.. |