Adamas Adalon® 805 PTFE, 40% Bronze

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Adamas
Trade Name Adalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 805 PTFE, 40% Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 3.07 - 3.10 g/cc
3.07 - 3.10 g/cc
ASTM D792
Water Absorption 0.020 %
0.020 %
ASTM D570
Deformation 7.0 - 9.9 %
7.0 - 9.9 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
7.0 - 10 %
7.0 - 10 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 58 - 62
58 - 62
ASTM D2240
Tensile Strength at Break >= 20.0 MPa
>= 2900 psi
ASTM D4745-11
Elongation at Break >= 200 %
>= 200 %
ASTM D4745-11
Coefficient of Friction, Dynamic 0.14 - 0.16
0.14 - 0.16
ASTM D1894
Coefficient of Friction, Static 0.16 - 0.18
0.16 - 0.18
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -140 °C
-220 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257