Material Notes:
PERMABOND® LH050 PURE anaerobic pipe sealant is single component paste that cures only when in contact with metal parts and oxygen is excluded. The sealant fills up the entire space between male and female parts, instantly sealing the connection for water, hydraulic fluids, air, gases and chemicals. Once cured, the cured anaerobic sealant typically exceeds the burst rating of the pipe and in addition it locks the pipes, plugs or fittings against vibration loosening. After cure, disassembly of fittings for maintenance is still possible using normal tools.Permabond® LH050 PURE pipe sealant performs well on most metals, particularly steel and brass. It provides an excellent alternative to pipe dopes and pipe tapes for sealing pipe joints. Another feature of PERMABOND® LH050 PURE is the ability to seal pipes that have not been fully seated. In piping systems, pipe joints must connect with other pipes and in the direction in which the joint must face may not allow the pipe to be fully seated. LH050 PURE will seal – even when the direction in which the pipe must face does not allow the complete seating of the threads. Anaerobic sealant will seal with simple hand assembly while still obtaining the seal of a fully torqued pipe joint. Features & Benefits: Full cure seal to the burst rating of pipe Easy to use and apply Directional freedom NSF/ANSI 61 Certified - Drinking Water System Components Does not contain solvents Excellent chemical and temperature resistance Cures at room temperature Will not shred, tear or cause blockages Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 250000 cP

@Temperature 25.0 °C
250000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.00 MPa
1020 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, handling strength
120 min

@Temperature 23.0 °C
2.00 hour

@Temperature 73.4 °F
M10 steel, handling strength
180 min

@Temperature 23.0 °C
3.00 hour

@Temperature 73.4 °F
Brass, working strength
180 min

@Temperature 23.0 °C
3.00 hour

@Temperature 73.4 °F
Zinc, handling strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
M10 steel, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Zinc, working strength
4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 20% at 200°C
Relative to 0°C
60% at 150°C
Relative to 0°C
85% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 3
M10 steel, prevail
4
M10 steel, break
UV Fluorescence No