Material Notes:
105C plug molding compound. UL recognized component for 94-5VA in all colors (3.0 mm min. thickness). UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.41 g/cc
1.37 - 1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 43 - 49
43 - 49
delayed; ASTM D-2240
55 - 61
55 - 61
ASTM D-2240
Tensile Strength, Yield 20.3 MPa
2950 psi
ASTM D-638
Elongation at Yield 280 %
280 %
ASTM D-638
100% Modulus 0.0138 GPa
2.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -11.0 °C
12.2 °F
ASTM D-746
Flammability, UL94 5VA

@Thickness >=3.00 mm
5VA

@Thickness >=0.118 in
All colors
Oxygen Index 31 %
31 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F