Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Conductive Carbon, Powder Modified
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.8 MPa
3300 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Yield Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1000 - 1.00e+6 ohm
1000 - 1.00e+6 ohm
ASTM D4496