Polymer Property : Tensile Strength, Ultimate = 22.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.8 MPa
3300 psi
ASTM D638
Multibase Multi-Pro® 4615 X White Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Ultimate 22.8 - 27.6 MPa
3300 - 4000 psi
ASTM D638
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Tensile Strength, Ultimate 22.8 MPa
3310 psi
ASTM D638
Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced  (discontinued **)
Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group.
Tensile Strength, Ultimate 22.8 MPa
3310 psi
ASTM D4745
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled  (discontinued **)
Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon.
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Vulcanized
KKPC KOSYN 1724 Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Vulcanized
KKPC KOSYN 1778K Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
KKPC KOSYN SOL 5990 Solution Styrene Butadiene Rubber (S-SBR)
Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It ..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
ASTM D638
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled
Conductive Carbon, Powder Modified
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Williams Advanced Alloys WS213 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate >= 22.8 MPa

@Thickness 3.17 mm
>= 3300 psi

@Thickness 0.125 in
ASTM D638
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene
Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
ASTM D638
Colorite Polymers 9533 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
ASTM D638
Colorite Polymers 9609 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Colorite Polymers 9611 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Colorite Polymers 9612 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Colorite Polymers 9811 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Colorite Polymers 9812 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
Tensile Strength, Ultimate 22.8 MPa
3310 psi
3M Jet-Weld™ TS-230 Adhesive
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Sprayable/extrudable grade with long set time ideal for bonding a wide variety of p..
Tensile Strength, Ultimate 22.8 MPa
3310 psi
ASTM D638
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 22.8 MPa
3300 psi
TM R050-36
Resinlab® EP1026HP Epoxy Adhesive
Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan..
Tensile Strength, Ultimate 22.8 MPa
3300 psi
Sylvin Technologies 6055 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.