Chosun Refractories BATN-3 Gas Purging Refractory

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories BATN-3 Gas Purging Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
Porosity 21 - 25 %
21 - 25 %
Mechanical Properties Metric English Comments
Compressive Strength <= 19.6 MPa
<= 2840 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 88 - 93 %
88 - 93 %
Descriptive Properties Value Comments
Main Application Porous Nozzle, Sharp and homogeneous pore size distribution
Permeability(?,cm/?,sec,h2o,cm) 1.3