Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
North Wood Plastics HDPE with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | <= 31.0 MPa | <= 4500 psi | ASTM D790 |
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled
(discontinued **) Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled Conductive Carbon, Powder Modified |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Spartech Royalstatâ„¢ R635 ABS/Polyolefin Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Techmer ES HiFill FR® PP CO E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Techmer ES HiFill FR® PP CO FR HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and CopolymerUL File Number: E157318Processing Method: Injection MoldingInformation provi.. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Techmer ES HiFill® PP GB40 40% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Washington Penn PPH4CF1 Polypropylene, 10% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Wash tubs.Data provided by Washington Penn Plastic Co., Inc. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | ASTM D790 |
Tipco Tipcolene® ISL 10 BX1 - 10% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow, Stiffness & Impact Strength 10% Mineral Reinforced, High Stiffness, High Impact PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
Indi.. |
|||
Flexural Yield Strength | 31.0 - 45.0 MPa @Temperature 260 - 260 °C |
4500 - 6530 psi @Temperature 500 - 500 °F |
Average value: 38.0 MPa Grade Count:4 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Yield Strength | 31.0 MPa | 4500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 31.0 - 186 MPa | 4500 - 27000 psi | Average value: 75.4 MPa Grade Count:18 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 31.0 - 220 MPa | 4500 - 31900 psi | Average value: 77.7 MPa Grade Count:74 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |