Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | |
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | |
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS FXC810MA is the grade code for the Marble effect in PC/ABS. Marble is part of the VisualFX portfolio, and it is offered in a range of colors simluating the Marble effect. High heat/good flow charact.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -30.0 °C |
8.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss a.. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 A |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9001-16H , 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D-256 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | Edgewise; ASTM D256 |
Haysite H722 Polyester, Glass Reinforced H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, .. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® ABS/PBT 1000 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® AE PC/ABS 7000-1 PC/ABS Engineered Resin Melt flow index may be specified. |
|||
Izod Impact, Notched | 4.27 - 4.81 J/cm | 8.00 - 9.00 ft-lb/in | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 22.8 °C |
8.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |