Techmer ES Electrablend® PC 04003 FR BK Stainless Steel Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer Techmer ES
Trade Name Electrablend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PC 04003 FR BK Stainless Steel Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 5.8 %
5.8 %
ASTM D638
Flexural Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 2.61 GPa
379 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
35.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 1000 ohm-cm
1.0 - 1000 ohm-cm
ASTM D257
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
FTMS 101B
Shielding Effectiveness 55 dB
55 dB
ASTM D4935