Polymer Property : Izod Impact, Unnotched = 4.43 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica..
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.43 J/cm

@Temperature 23.0 °C
8.30 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Izod Impact, Unnotched 4.43 J/cm

@Temperature 23.0 °C
8.30 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
Izod Impact, Unnotched 4.43 J/cm

@Temperature 23.0 °C
8.30 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC 04003 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC 05004 FR Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.17 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr..
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DDF029 PC (Asia Pacific)
LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant, Glass Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66
LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific)
LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DDF029 PC
LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant.
Izod Impact, Unnotched 4.43 J/cm

@Thickness 3.18 mm
8.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant  (discontinued **)&l
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Izod Impact, Unnotched 4.43 J/cm
8.30 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.