Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 0.10 sec | 0.10 sec | (Mil-B-81705C), 50% RH, 5000 kV to 50 kV |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® ABS 04001 BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Static Decay | 0.10 sec | 0.10 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Static Decay | 0.10 sec | 0.10 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific) Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN.. |
|||
Static Decay | 0.10 sec | 0.10 sec | 5000V to <50V; FTMS101B |
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific) Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications. |
|||
Static Decay | <= 0.10 sec @Temperature 23.0 °C |
<= 0.10 sec @Temperature 73.4 °F |
50% RH; JIS L1049 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | FTMS 101B |
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr.. |
|||
Static Decay | 0.10 sec | 0.10 sec | FTMS-101C; 12% R.H. (-5000 V to -50 V) |
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy Stat-Rite® M-690 is a static dissipative PETG alloy. Stat-Rite® M-690 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Static Decay | 0.10 sec | 0.10 sec | Charged Plate Monitor, 50% RH (+1000 V to 100 V) |
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p.. |
|||
Static Decay | 0.10 sec | 0.10 sec | Charged Plate Monitor, 50% RH (+1000 V to 100 V) |
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD .. |
|||
Static Decay | 0.10 sec | 0.10 sec | Charged Plate Monitor; 50% R.H. MD, (+1000 V to 10 V) |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive) Non-sloughing, carbon-fiber-filled material with high strength and stiffness; easily machined.Information provided by Westlake Plastics. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Absylux® CN-P Acrylonitrile-Butadiene-Styrene (conductive) Carbon-powder-filled conductive material with high strength and stiffness, and relatively high impact strength. This material is easily machined and fabricated into close tolerance finished parts. .. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive) Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Propylux® CN-P Polypropylene (conductive) Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Tempalux® CN-F Polyetherimide (conductive) Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resist.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Zelux® CN-P Polycarbonate (conductive) Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Zelux® CN-SS Polycarbonate (conductive) CN-SS is filled with small non-sloughing stainless steel fibers. Has high flexural strength and good thermal stability to 275F. The CN-SS material has excellent impact strength. Information provid.. |
|||
Static Decay | <= 0.10 sec | <= 0.10 sec | 15% RH; MIL-B-81705-B |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Static Decay | 0.10 sec | 0.10 sec | (+1000 V to 100 V) |
Lubrizol Stat-Rite® SIS535 Static Control System Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma.. |