Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radiflam® S RV250FR (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® S RV250FR (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
Water Absorption 2.5 %
2.5 %
Moisture Absorption at Equilibrium 1.1 %
1.1 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
Elongation at Break 1.8 %
1.8 %
Tensile Modulus 14.3 GPa
2070 ksi
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Users viewing this material also viewed the following: