Material Notes:
CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Thermoformed hot fill applications Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Elongation at Break 30 %
30 %
50 mm/min; ASTM D638
Flexural Strength 49.0 MPa

@Thickness 3.20 mm
7110 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.77 GPa

@Thickness 3.20 mm
256 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.150 J/cm

@Thickness 3.20 mm
0.281 ft-lb/in

@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 3.00 J/cm

@Thickness 3.20 mm
5.62 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Vicat Softening Point 101 °C
214 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Haze 5.5 %

@Thickness 1.00 mm
5.5 %

@Thickness 0.0394 in
SPL test method
Transmission, Visible 86 %

@Thickness 1.00 mm
86 %

@Thickness 0.0394 in
SPL test method
Processing Properties Metric English Comments
Melt Temperature <= 220 °C
<= 428 °F
Mold Temperature 40.0 - 50.0 °C
104 - 122 °F
Users viewing this material also viewed the following: