Polymer Property : Tensile Strength at Break = 34.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.3 MPa

@Thickness 2.00 mm
4970 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Tensile Strength at Break 34.3 MPa

@Thickness 2.00 mm
4970 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
LG Chemical KEYFLEX BT 1155D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Tensile Strength at Break 34.3 MPa
4970 psi
ASTM D638
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene
HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applic..
Tensile Strength at Break 34.3 MPa
4970 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced
Anti-staticInformation provided by Samsung Cheil Industries.
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Strength at Break 34.3 MPa
4970 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 34.3 MPa
4970 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced
Anti-staticInformation provided by Samsung Cheil Industries.
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Strength at Break 34.3 MPa
4970 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 256 Toughened Polystyrene
Characteristics Superior flexibility Good ball drop strength Excellent clarity Easy flow Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric ..
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 265 Toughened Polystyrene
CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther..
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 266 Toughened Polystyrene
CharacteristicsGood stiffness Excellent toughness High flow Excellent clarity Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric instruments ..
Tensile Strength at Break 34.3 MPa
4970 psi
50 mm/min; ASTM D638
Supreme Petrochem SPEXP 44 Antistatic Polystyrene
Characteristics Easy flow Good transparency Very good flexibility Processing Extrusion Applications Transparent profiles for electrostatic dissipative packaging of small electronic components such..
Tensile Strength at Break 34.3 MPa
4970 psi
ASTM D3759
3M 3340 HVAC Construction
Aluminum foil tape, for use with rigid and flexible ducts. UL 181 A-P and 181 B-FX Listed.Information provided by 3M
Tensile Strength at Break 34.3 MPa
4970 psi
ASTM D3759
3M 33801 Premium Performance Aluminum Foil Tape
High temperature acrylic adhesive of 425°F. UL 723 ClassifiedInformation provided by 3M