Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP640N Injection Molding Grade Polypropylene Moplen HP640N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640N is a homopolymer particularly suitable for injection molding.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer Titanpro® PM803 is a high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | |
Kraton® G1651 + PPE blend (10/90) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
Hannam Chemical Hanalac 795 ABS, Pipe Grade Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN173HI3R High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
Kostat BK-STAT 7048BK ABS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced Used in electric goods etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced Used in electric goods etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 266 Toughened Polystyrene CharacteristicsGood stiffness Excellent toughness High flow Excellent clarity Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric instruments .. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 6131 XF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | Procedure B, Test Method I(chs 0.05 in/min); ASTM D790 |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron AN-312 Flame Retardant ABS Grade |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade Antistatic Cop Sleeves ApplicationInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP EXP 31 Toughened Polystyrene Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form.. |