Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 101 °C | 214 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir N 1782 Polystyrene General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 0.125 inch bar, 1 Kg; ASTM D1525 |
Network Polymers SAN 277 Blue Tint Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate A; 4 mm thick;10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific) Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance.. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
Ineos Nova 731G High Impact Polystyrene
(discontinued **) Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs .. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50 N - 120°C/h; ISO 306/B120 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Vicat Softening Point | 101 °C | 214 °F | ISO |
I. Stern N2380 High Heat Crystal Polystyrene Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h 50N |
Ineos ABS Lustran® Elite HH 1827 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Vicat Softening Point | 101 °C @Load 5.10 kg |
214 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Vicat Softening Point | 101 °C | 214 °F | ISO R-306 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 101 °C | 214 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 101 °C | 214 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
Sumitomo Chemical Sumipex® LG2 Acrylic Resin, High Flow Product CharacteristicsHigh FlowInformation provided by Calsak Corporation |
|||
Vicat Softening Point | 101 °C | 214 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP 265 Toughened Polystyrene CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther.. |
|||
Vicat Softening Point | 101 °C | 214 °F | |
UBE UBEPOL BR13HB HIPS (n-DM =0.03 wt %) Description: UBEPOL-BR13HB is characterized by its low solution viscosity compared with conventional grades and short dissolution time in styrene monomer. Its main merits are as follows:Short dissol.. |
|||
Vicat Softening Point | 101 °C | 214 °F | |
UBE UBEPOL BR13HB HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBEPOL-BR13HB is characterized by its low solution viscosity compared with conventional grades and short dissolution time in styrene monomer. Its main merits are as follows:Short dissol.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h 50N |
Covestro Bayblend® FR 3001 Polycarbonate + ABS Blend Key Features:Flame retarding agentUnfilledFlame retardantSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and hydrolysis resistance antimony-, chlorine- and bromine-free flame retardant.. |
|||
Vicat Softening Point | 101 °C @Load 1.00 kg, Thickness 3.17 mm |
214 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers SAN 260 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 101 °C | 213 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
Bapolene® 1072 Polyethylene, Injection Grade A high flow general purpose injection molding resin with good gloss, toughness and stress crack resistance. This product meets FDA standards for food contact applications.Applications: Housewares, .. |
|||
Vicat Softening Point | 101 °C | 213 °F | ASTM D1525 |
Americas Styrenics EB6755 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Vicat Softening Point | 101 °C | 214 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D648 |
Amco Amalloy® B1017 Polymer Alloy Amco Amalloy B1017 is a clear performance copolymer with exceptional clarity and toughness.High melt-flow, very clear.Information provided by Amco Plastic Materials. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 171 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high .. |
|||
Vicat Softening Point | 101 - 102 °C | 214 - 216 °F | Average value: 101 °C Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |