Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Supreme Petrochem SC 201E General Purpose Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Supreme Petrochem LTD
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Supreme Petrochem SC 201E General Purpose Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CharacteristicsVery high molecular weight High heat grade Good melt strength Good clarity and mechanical strengthProcessing Extrusion MoldingApplicationsExtruded embossed sheets, OPS, foamed meat trays, insulation board Food and medical applications like disposable pipette, tablet packaging bottles, ampoule trays, caps & closuresMaterial Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.0 MPa
7540 psi
50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ASTM D638
Flexural Strength 97.1 MPa

@Thickness 3.20 mm
14100 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 2.94 GPa

@Thickness 3.20 mm
427 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.180 J/cm

@Thickness 3.20 mm
0.337 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
189 °F
ASTM D648
Vicat Softening Point 106 °C
223 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Users viewing this material also viewed the following: