Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Sumikon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. Typical applications include brush holders, housings, and heat insulators.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
Bulk Density 0.800 g/cc
0.0289 lb/in³
ASTM D1895
Bulk Factor 2.3
2.3
ASTM D1895
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D6289
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 124 MPa
18000 psi
ASTM D638
Tensile Modulus 17.9 GPa
2600 ksi
ASTM D638
Flexural Strength 200 MPa
29000 psi
ASTM D790
Compressive Strength 289 MPa
41900 psi
ASTM D695
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
Maximum Service Temperature, Air 150 °C

@Thickness 3.00 mm
302 °F

@Thickness 0.118 in
UL Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.3

@Frequency 1e+6 Hz
4.3

@Frequency 1e+6 Hz
ASTM D150
4.7

@Frequency 1000 Hz
4.7

@Frequency 1000 Hz
ASTM D150
5.1

@Frequency 60 Hz
5.1

@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm
400 kV/in
Step by Step; ASTM D149
17.7 kV/mm
450 kV/in
Short Time; ASTM D149
Dissipation Factor 0.010

@Frequency 1e+6 Hz
0.010

@Frequency 1e+6 Hz
ASTM D150
0.030

@Frequency 1000 Hz
0.030

@Frequency 1000 Hz
ASTM D150
0.050

@Frequency 60 Hz
0.050

@Frequency 60 Hz
ASTM D150