Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel Hysol EA 9696 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9696 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Second generation, moisture-resistant, toughened 250°F / 121°C service, modified epoxy film. Qualified to BMS 5-101 and BMS 5-129. Data from .060 psf, 300 g / m2.Applications: Composite Bonding Metal and Honeycomb Bonding Composite Surfacing
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 9.00 MPa
1310 psi
Flatwise
Adhesive Bond Strength 13.8 MPa

@Temperature 121 °C
2000 psi

@Temperature 250 °F
Lap Shear
41.3 MPa

@Temperature 25.0 °C
5990 psi

@Temperature 77.0 °F
Lap Shear
48.3 MPa

@Temperature -55.0 °C
7010 psi

@Temperature -67.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 110
at 25°C
Out-Time (days) 60
at 25°C