Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYshine PBT D223 GF20 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF10030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | 0.125inch wall |
Spartech PP5430 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Plenco 5118 Phenolic, Granular, Injection Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber Heat stabilized 35% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB300G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB310G6 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB321I6 Nylon 6, 30% Glass Fiber and Mineral 30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ISO 2577 |
Polyram PlusTek RA300G7 Nylon 6.6 for Injection Molding, 35% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 35% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AR-37 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell BR-17 Nylon 6, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell BT-37 Nylon 6, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Ashley Polymers Ashlene® 990L-30G Nylon 610, 30% Glass Reinforced 30% glass reinforced for excellent dimensional stability and low water absorption.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |