Polymer Property : Compressive Strength = 289 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 289 MPa
41900 psi
ASTM D695
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade
Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s..
Compressive Strength 289 MPa
41900 psi
ASTM D695
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic
Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in ..