Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate

Category Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP), Cast, Mineral Filler , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MIG.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
ASTM D792
Apparent Bulk Density 0.810 g/cc
0.0293 lb/in³
Water Absorption 0.50 %
0.50 %
48 hours, 50°C. ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Compression Molding. ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Flexural Yield Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Compressive Yield Strength 145 MPa
21000 psi
ASTM D695
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 130 °C
266 °F
UL temperature Index, UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 274 °C
525 °F
ASTM D648A
UL RTI, Electrical 130 °C
266 °F
UL temperature Index, UL 746B
UL RTI, Mechanical with Impact 130 °C
266 °F
UL temperature Index, UL 746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL temperature Index, UL 746B
Oxygen Index 23 %
23 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 4.1

@Frequency 1e+6 Hz
4.1

@Frequency 1e+6 Hz
Wet
4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Wet
Dielectric Strength 14.0 kV/mm
356 kV/in
Wet, step-by-step. ASTM D149
15.0 kV/mm
381 kV/in
Wet, short term. ASTM D149
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Wet; ASTM D150
0.025

@Frequency 1e+6 Hz
0.025

@Frequency 1e+6 Hz
Wet; ASTM D150
Arc Resistance 175 sec
175 sec
ASTM D495
Comparative Tracking Index >= 600 V
>= 600 V
UL746A, ASTM D3638
Processing Properties Metric English Comments
Processing Temperature 160 - 180 °C
320 - 356 °F
Mold temperature