Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1413-t1 Polyolefin TPO Granules, Dark Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1452 Polyolefin TPO Granules, Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 140 - 180 °C | 284 - 356 °F | |
Taiwan Sheen Soon Sheenthane® A8361E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Processing Temperature | 140 - 180 °C | 284 - 356 °F | Films Die Head |
EMS-Griltech Griltex® 1A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 417 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:SheathingInformation provided by Fainplast Compounds |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 039/4H Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 211 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo.. |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 225F Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, high flexibilityInformation provided by Fainplast Compounds |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 045/11 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Membranes |
Lucobit Lucofin® 1412-t1 Polyolefin TPO Granules, Light Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |