Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 274 °C | 525 °F | ASTM D648A |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 274 °C | 525 °F | ASTM D648A |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 274 - 290 °C | 525 - 554 °F | Average value: 284 °C Grade Count:10 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 274 °C | 525 °F | ASTM D648A |
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI.. |