Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 101R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 121R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 201R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Super mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3414R PC 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® FXD121R PC (Asia Pacific) Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 141 PC General purpose polycarbonate with melt flow rate of 10.5. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 141R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | |
Glastic Laminates/Shapes 1603-2A Fiberglass-Reinforced Polyester Standoff Insulator Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL temperature Index, UL 746B |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | |
Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR Information provided by Samsung Cheil Industries. |