Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Zylar 960 MBS

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Styrolution
Trade Name Zylar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Zylar 960 MBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injection molded applications.Exceptional toughnessLow densityEase of processingGamma & ETO sterilizableMeets USP XXIII specifications for Class VI plasticsInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D 792
Water Absorption at Saturation 0.10 %

@Temperature 23.0 °C
0.10 %

@Temperature 73.4 °F
ASTM D 570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D 955
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62
62
ASTM D 785
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D 638
Elongation at Break 70 %
70 %
ASTM D 638
Tensile Modulus 1.72 GPa
250 ksi
ASTM D 638
Flexural Strength 42.7 MPa
6200 psi
ASTM D 790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D 790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D 256
Gardner Impact 19.2 J
14.2 ft-lb
ASTM D 5420
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 249 °C
480 °F
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
Vicat Softening Point 93.9 °C

@Load 1.02 kg
201 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
Sodium D Line; ASTM D 542
Haze 2.0 %
2.0 %
ASTM D 1003
Transmission, Visible >= 91 %

@Wavelength 550 nm
>= 91 %

@Wavelength 550 nm
ASTM D 1003
Processing Properties Metric English Comments
Melt Temperature 204 - 238 °C
400 - 460 °F
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Drying Temperature 65.6 °C

@Time 7200 sec
150 °F

@Time 2.00 hour