Thermal Properties Metric English Comments
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet)
Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet)
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® CM HPV PEEK Polyetheretherketone; PTFE, Graphite, and Carbon Fiber Filled Bearing Grade, compression molded (ASTM Product Data Sheet)
Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet)
Maximum Service Temperature, Air 249 °C
480 °F
Continuous
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet)
Maximum Service Temperature, Air 249 °C
480 °F
Quantum PEEK 30% Carbon Filled
Information provided by Quantum Advanced Engineering Plastics
Maximum Service Temperature, Air 249 °C
480 °F
Technetics Group Amicon™ PEEK  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Maximum Service Temperature, Air 249 °C
480 °F
Technetics Group Amicon™ PEEK 30% Glass Filled  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Maximum Service Temperature, Air 249 °C
480 °F
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Maximum Service Temperature, Air 249 °C
480 °F
Styrolution Zylar 650 MBS
Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact..
Maximum Service Temperature, Air 249 °C
480 °F
Styrolution Zylar 960 MBS
ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec..
Maximum Service Temperature, Air 249 °C
480 °F
Styrolution Clearblend 145 MBS
Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution
Maximum Service Temperature, Air 249 °C
480 °F
Styrolution Clearblend 165 MBS
CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.Exceptional toughnessLow densityEase of processingLow moisture absorptionInforma..
Maximum Service Temperature, Air 249 °C
480 °F
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..
Maximum Service Temperature, Air 249 °C
480 °F
Long Term
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho..
Maximum Service Temperature, Air 249 °C
480 °F
Quantum PEEK
Information provided by Quantum Advanced Engineering Plastics
Copyright © lookpolymers.com All Rights Reserved