Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 26.7 - 54.4 °C | 80.1 - 130 °F | |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.1 - 130 °F | |
PolyOne Trilliant™ HC 5410-0030RS Natural Polyethylene, High Density (HDPE) Information provided by PolyOne |
|||
Mold Temperature | 37.8 - 54.4 °C | 100 - 130 °F | |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Mold Temperature | 37.8 - 54.4 °C | 100 - 130 °F | |
Northstar Polymers MPS-F06B Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Mold Temperature | 37.8 - 54.4 °C | 100 - 130 °F | |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.1 - 130 °F | |
PolyOne Edgetek® PE-30GF/000 Polyethylene, High Density (HDPE) Information provided by PolyOne |
|||
Mold Temperature | 37.8 - 54.4 °C | 100 - 130 °F | |
PolyOne Edgetek® AS-03CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
PolyOne Edgetek® PE-40GF/000 NATURAL High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedNaturalPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 32.2 - 54.4 °C | 90.0 - 130 °F | |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
Styrolution Zylar 960 MBS ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec.. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
Styrolution Clearblend 145 MBS Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
Styrolution Clearblend 165 MBS CLEARBLEND 165 is an impact modified styrene acrylic copolymer blend with excellent clarity and outstanding toughness.Exceptional toughnessLow densityEase of processingLow moisture absorptionInforma.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Mold Temperature | 43.3 - 54.4 °C | 110 - 130 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
PolyOne Edgetek® PE-25CF/000 High Density Polyethylene (HDPE), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
PolyOne Stat-Tech™ AS-30GF/000 SD Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedAntistaticInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
PolyOne Edgetek® PE-30GF/000 WHITE High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedWhitePolyOne First ChoiceInformation provided by PolyOne Corporation. |