Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 74.0 - 100 MPa | 10700 - 14500 psi | Average value: 87.3 MPa Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Ball Indentation Hardness | 74.0 MPa | 10700 psi | DIN 53456 |
Global PP-2300-NC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Ball Indentation Hardness | 74.0 MPa | 10700 psi | ISO 2039-1 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Ball Indentation Hardness | 74.0 MPa | 10700 psi | H 358/30; Ø 50x4mm; ISO 2039-1 |
SYNTHOS Forsan® 846 Acrylonitrile Butadiene Styrene (ABS) High impact, medium flow, glossy, suitableApplications: General purpose, transport packaging, furniture, leisure time equipmentContainers, suitcases, profiles, ABS sheets, skis, helmets, garden equi.. |
|||
Ball Indentation Hardness | 74.0 MPa @Load 36.5 kg, Time 30.0 sec |
10700 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Polystyrol 495 F GR 2 PS Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ.. |
|||
Ball Indentation Hardness | 74.0 MPa | 10700 psi | ISO 2039-1 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Ball Indentation Hardness | 74.0 MPa | 10700 psi | ISO 2039-1 |
Styrolution PS 495N HIPS Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor.. |
|||
Ball Indentation Hardness | 74.0 MPa @Load 36.5 kg, Time 30.0 sec |
10700 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |