Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B BT Polyethylene Terephthalate FeaturesPBT basic type for injection moulding. Melt is characterized by outstanding fluidity, which enables injection moulding of complicated and divided products also on multiple moulds. Anisotro.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -20.0 °C |
61.9 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B BT Polyethylene Terephthalate FeaturesPBT basic type for injection moulding. Melt is characterized by outstanding fluidity, which enables injection moulding of complicated and divided products also on multiple moulds. Anisotro.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -20.0 °C |
61.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -20.0 °C |
61.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -20.0 °C |
61.9 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 1100 000000 PBT PBT, non-reinforced, extrusion, injection molding, improved flowability |
|||
Charpy Impact Unnotched | <= 13.0 J/cm² @Temperature -30.0 °C |
<= 61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Polystyrol 495 F GR 2 PS Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Novamid® 1013G45 1 NA PA6-GF45 45% Glass Reinforced, Injection Molding |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45 45% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
DIN ISO 179 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2002 25% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, Conditioned Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, Conditioned Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 562E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo.. |