Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East) 19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC B5429/B5429A High Density Polyethylene for Blow Molding Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades.. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm |
3.37 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **) A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | >= 1.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 3.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm |
3.37 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Styrolution Polystyrol 495 F GR 2 PS Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 0.000 °C |
3.37 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber 30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P40B03 Copolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber A CHEMICALLY COUPLED 40% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-G15 PTFE Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |