Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | 100V |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Kingfa HP-126 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Kingfa JE2-R2 ABS/PBT Alloy Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Kingfa PA6-G15 15% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 60093 |
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm @Temperature 23.0 °C |
1.00e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 60093 |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm @Temperature 23.0 °C |
1.00e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Covestro Apec® FR1892 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 60093 |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 60093 |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D149 |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm @Temperature 100 °C |
>= 1.00e+16 ohm-cm @Temperature 212 °F |
|
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Eurotec® Tecodur® PB70 GR30 NL PBT 30% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Beijing Chemical Industry KAIFA® 201-G30 PBT Resin 30% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |