Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Royalite R12 ABS General Purpose Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Royalite R12 ABS General Purpose Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: General Purpose SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.08 g/cc
1.02 - 1.08 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Flexural Yield Strength 61.4 MPa
8900 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
73°F; ASTM D256
0.961 J/cm

@Temperature -28.9 °C
1.80 ft-lb/in

@Temperature -20.0 °F
ASTM D256
Impact Test 27.1 J

@Temperature 22.8 °C
20.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 75.6 - 101 µm/m-°C

@Temperature 20.0 °C
42.0 - 56.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Descriptive Properties Value Comments
Flammability Passes
MVSS (Motor Vehicle Safety Standard) 302
Users viewing this material also viewed the following: