Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 61.4 - 137 MPa | 8900 - 19900 psi | Average value: 102 MPa Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Flexural Yield Strength | 61.4 MPa | 8900 psi | ASTM D790 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |