Mechanical Properties Metric English Comments
Flexural Yield Strength 61.4 - 137 MPa
8900 - 19900 psi
Average value: 102 MPa Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
Flexural Yield Strength 61.4 MPa
8900 psi
ASTM D790
Spartech Royalite R12 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.