Mechanical Properties Metric English Comments
Impact Test 27.1 J

@Temperature 22.8 °C
20.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R570 FR-ABS Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Impact Test 27.1 J

@Temperature 22.8 °C
20.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R12 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.