Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP552N Fiber (Staple) Grade Polypropylene Moplen HP552N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552N is a homopolymer selected by customers for use in high speed.. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP562T Fiber (Spunbond) Grade Polypropylene Moplen HP562T is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562T is a homopolymer particularly suitable f.. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
PolyMirae Moplen HP640R Injection Molding Grade Polypropylene Moplen HP640R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640R is a homopolymer particularly suitable for injection molding.. |
|||
Tensile Strength, Yield | 37.3 MPa @Thickness 3.20 mm |
5400 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Spartech SP-9020 Premium ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8009 FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® EG-0763 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM Data |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
PlastxWorld CEVIAN® E80 ABS Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 5140H Compression Molding Polypropylene HomopolymerApplications: Compression Molded Caps and Closure ApplicationsFormolene 5140H DEVELOPMENTAL is a polypropylene homopolymer designed and formulated for compression molded caps and closure .. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
Cheng Yu Plastic PP227 Flame Retardant Polypropylene, Medium Impact |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
CPC - Vycom PROTEC® Homopolymer Polypropylene Protec HP is a high corrosion resistant polypropylene material which exhibits excellent tensile strength and stiffness at elevated temperatures. Homopolymer polypropylene possesses excellent resista.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA T-105 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP30-1200S Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | 2 in/min (50 mm/min); ASTM D-638 |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Tensile Strength, Yield | 37.3 MPa | 5400 psi | ASTM D638 |
Cheng Yu Plastic BK1022 Electric Conducting Polypropylene, Injection |
|||
Tensile Strength, Yield | 37.3 MPa @Thickness 3.20 mm |
5400 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Albis Plastics ASA 02A MR20 , 20% Mineral Filled
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Tensile Strength, Yield | 37.2 MPa | 5400 psi | ASTM D638 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |