Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Mineral Reinforced
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspect and Dimensional stability Applications: TECHNYL B 738 MX15 Cinza 3279 is indicated for automotive and electrical industry. Ex.: Wheel CoverInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183/A
Water Absorption 1.17 %

@Temperature 23.0 °C,
Time 86400 sec
1.17 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.0 MPa
8560 psi
ISO R 527
Elongation at Break 3.0 %
3.0 %
ISO R 527
Tensile Modulus 4.30 GPa
624 ksi
ISO R 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 3.70 GPa
537 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 243.5 °C
470.3 °F
Processing Properties Metric English Comments
Feed Temperature 250 - 260 °C
482 - 500 °F
Nozzle Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Descriptive Properties Value Comments
Compression Zone 260-280°C
Mixing Zone 250-270°C
Users viewing this material also viewed the following: