Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® A 221 Natural FA PA66, DRY Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® A 222 Black 1N PA66, DRY Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® A 246M PA66, DRY Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay Technyl® A218 Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY Description: Polyamide 6, reinforced with 11% of glass fiber, with high impact resistance, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® C 246SI V11 has good mech.. |
|||
Feed Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
  Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Feed Temperature | 250 - 280 °C | 482 - 536 °F | |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |