Polymer Property : Feed Temperature = 482 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)  (discontin
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY
Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® A 221 Natural FA PA66, DRY
Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® A 222 Black 1N PA66, DRY
Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay TECHNYL® A 225F PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® A 246M PA66, DRY
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Feed Temperature 250 - 260 °C
482 - 500 °F
Solvay TECHNYL® B 216 Natural D PA66/6, DRY
Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,..
Feed Temperature 250 - 260 °C
482 - 500 °F
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY
Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:..
Feed Temperature 250 - 270 °C
482 - 518 °F
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu..
Feed Temperature 250 - 260 °C
482 - 500 °F
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled
Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY
Description: Polyamide 6, reinforced with 11% of glass fiber, with high impact resistance, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® C 246SI V11 has good mech..
Feed Temperature 250 - 260 °C
482 - 500 °F
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY
Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)  (discontinu
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM  (discontinued **)<
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)  
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM  (discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)  
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)  (discontinued **
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Feed Temperature 250 - 280 °C
482 - 536 °F
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..