Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.70 GPa | 537 ksi | |
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | |
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Nilit FRIANYL A63 SG30 Nylon 6.6 for injection molding, 30% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYsan PN127 Styrene Acrylonitrile Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 513RS PC (Europe-Africa-Middle East) LEXAN 513RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 - 12.4 GPa | 537 - 1800 ksi | Average value: 7.80 GPa Grade Count:122 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2mm/min; ASTM D790 |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Solvay TECHNYL® B 738 MX15 Grey 3279 PA66/6, 15% mineral filled Description: TECHNYL B 738 MX15 Grey 3279 is a Polyamide 6.6, with 15% of mineral filler. Colors: GreyAvailable in: Latin AmericaMain Properties: ? Good Mechanical Properties, Good Superficial Aspec.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK) KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 136F4Q32 Nylon 6, 20% Glass Fiber SAXAMID 136F4Q32 is a high impact-modified polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | Tangent |
Schmelzer Industries Pearlveil 110-10 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D 790 |
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |