Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance molding using conventional molding equipment.Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI UnitsData provided by Chevron Phillips Chemical Company LP.Solvay Specialty Polymers has acquired the Ryton product line.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 170 MPa
24700 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
ASTM D638
Flexural Yield Strength 240 MPa
34800 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM D790
Compressive Yield Strength 275 MPa
39900 psi
ASTM D695
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.30 J/cm
9.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 100 - 200 °C
6.67 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
12.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
6.67 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
95.0 µm/m-°C

@Temperature 100 - 200 °C
52.8 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
UL Temperature Index 200 / 220 per UL746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Annealed 2 hr @ 200°C; ASTM D649
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1000 Hz
4.0

@Frequency 1000 Hz
ASTM D150
4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 sec
125 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
UL 746A