Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.67 µin/in-°F @Temperature 32.0 - 212 °F |
|
Kennametal Stellite Stellite® STAR with P/M Processing Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 38.0 - 200 °C |
6.67 µin/in-°F @Temperature 100 - 392 °F |
|
Latrobe LSSâ„¢ Vertex Tool Steel TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the micros.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 21.0 - 427 °C |
6.67 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe CBS-50™ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 24.0 - 204 °C |
6.67 µin/in-°F @Temperature 75.2 - 399 °F |
|
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 600 °C |
6.67 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 - 15.0 µm/m-°C @Temperature -40.0 - 125 °C |
6.67 - 8.33 µin/in-°F @Temperature -40.0 - 257 °F |
X/Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |
|||
CTE, linear | 12.0 - 15.0 µm/m-°C @Temperature -40.0 - 125 °C |
6.67 - 8.33 µin/in-°F @Temperature -40.0 - 257 °F |
X/Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 100 - 200 °C |
6.67 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 24.0 - 204 °C |
6.67 µin/in-°F @Temperature 75.2 - 399 °F |
|
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 21.0 - 427 °C |
6.67 µin/in-°F @Temperature 69.8 - 801 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
CTE, linear | 12.0 - 15.5 µm/m-°C @Temperature -40.0 - 125 °C |
6.67 - 8.62 µin/in-°F @Temperature -40.0 - 257 °F |
X/Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |