Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C @Temperature 400 °C |
6.67 µin/in-°F @Temperature 752 °F |
|
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 100 - 200 °C |
6.67 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Kennametal Stellite Nucalloy® 488 High-Silicon Nickel-Base Hardfacing Alloy Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness and toughness, similar to the cobalt base alloys . B.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 300 °C |
6.67 µin/in-°F @Temperature 572 °F |
|
MarkeTech Repton 914 Magnesia MgO REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 38.0 - 200 °C |
6.67 µin/in-°F @Temperature 100 - 392 °F |
|
Latrobe LSSâ„¢ Vertex Tool Steel TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the micros.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 0.000 - 500 °C |
6.67 µin/in-°F @Temperature 32.0 - 932 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 21.0 - 427 °C |
6.67 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe CBS-50™ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 24.0 - 204 °C |
6.67 µin/in-°F @Temperature 75.2 - 399 °F |
|
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
|
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Annealed, 1.27 mm Strip Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 100 - 200 °C |
6.67 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 21.0 - 427 °C |
6.67 µin/in-°F @Temperature 69.8 - 801 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 300 °C |
6.67 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |