Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Thermal Conductivity | 0.330 - 4.00 W/m-K | 2.29 - 27.8 BTU-in/hr-ft²-°F | Average value: 0.462 W/m-K Grade Count:60 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/CF/15/TF/20/BK Polyamide 66, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ASTM E1530 |
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ASTM E1530 |
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | Silicone Property; ASTM E 1530 |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® R36211A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primerDesign/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: St.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3K PA6 (Conditioned) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3K BK 00464 PA66 (Conditioned) Description: Easy flowing injection-molding grade for fast processing. Uses include highly stressed technical parts such as bearings and gear wheels; also electrically insulating parts such as termi.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3W PA66 (Conditioned) Description: Free-flowing, heat aging resistant and rapidly processable grade for technical parts subject to high stress such as bearings and bearing cages, gearwheels and spool bodies.Information p.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3K BK00464 PA6 (Dry) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Thermal Conductivity | 0.330 W/m-K | 2.29 BTU-in/hr-ft²-°F | |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten.. |